22041 I-ejenti Yokulinganisa (Ye-acrylic fiber)
Izici & Izinzuzo
- Ayiqukethe i-benzalkonium chloride.
- Ingenza odayi be-cationic kancane kancane idayi kumazinga okushisa ahlukene futhi ilungise kahle izinga lokudaya.
- Inempahla ebambezelekayo futhi idlulisa impahla kokubili.
- Ukusebenza kancane kancane.Inikeza izindwangu ezithatha udayi eziphezulu nokushesha okuhle.
Izakhiwo Ezijwayelekile
Ukubukeka: | Uketshezi olusobala olungenambala ukuya kokuphuzi |
I-Ionity: | I-Cationic |
Inani le-pH: | 4.0±1.0 (1% isixazululo esinamanzi) |
Ukunyibilika: | Incibilika emanzini |
Okuqukethwe: | 19~20% |
Isicelo: | Imicu ye-Acrylic |
Iphakheji
Umphongolo wepulasitiki ongu-120kg, ithangi le-IBC kanye nephakheji elenziwe ngezifiso liyatholakala ukuze likhethwe
AMACEBISO:
Ukudaya okuqhubekayo
Ukudaya okuqhubekayo kuyinqubo lapho ukudaya indwangu kanye nokulungiswa kwedayi kwenziwa ngokuqhubekayo ekusebenzeni okukodwa ngesikhathi esisodwa.Lokhu ngokwesiko kwenziwa kusetshenziswa isistimu yolayini wokukhiqiza lapho amayunithi ehlanganiswa abe yimigqa yezinyathelo zokucubungula ezilandelanayo;lokhu kungabandakanya kokubili ukwelashwa kwangaphambili nangemuva kokudaywa.Indwangu ivame ukucutshungulwa ngobubanzi obuvulekile, ngakho-ke kufanele kuthathwe ukunakekelwa ukuze unganweli indwangu.Isivinini sokugijima kwendwangu sichaza isikhathi sokuhlala sendwangu ngeyunithi ngayinye yokwelapha, nakuba izikhathi zokuhlala zingandiswa ngokusebenzisa ukuthutha kwendwangu yohlobo lwe-'festoon'.Ububi obuyinhloko bokucubungula okuqhubekayo ukuthi noma yikuphi ukuwohloka kwemishini kungabangela indwangu eyonakele ngenxa yezikhathi zokuhlala ngokweqile kumayunithi athile ngenkathi ukuwohloka kulungiswa;lokhu kungaba yinkinga ethile lapho kusetshenziswa ama-stenter asebenza emazingeni okushisa aphezulu njengoba izindwangu zingashintsha umbala kakhulu noma zishiswe.
Ukufakwa kukadayi kungenziwa ngokufakwa ngqo, lapho utshwala obudayi bufuthwa khona noma buphrintwe ku-substrate, noma ngokucwiliswa okuqhubekayo kwendwangu endaweni yokudaya kanye notshwala obudayi obudlulele bususwe ngama-rollers (padding).
Ukupakisha kubandakanya ukudlulisa i-substrate ebhodweni lephedi elinotshwala obudayi.Kubalulekile ukuthi i-substrate imanziswe kahle njengoba idlula otshwaleni obudayi ukuze kuncishiswe ukungahleleki.Inani lotshwala bedayi eligcinwe yi-substrate ngemva kokucindezela lilawulwa ukucindezela kwama-rollers okucindezela kanye nokwakhiwa kwe-substrate.Inani lotshwala obugciniwe libizwa ngokuthi “cosha”, ukubuthwa okuncane kuyathandeka njengoba lokhu kunciphisa ukufuduka kotshwala obudayi ku-substrate futhi konga amandla ngesikhathi somiswa.
Ukuze uthole ukulungiswa okufanayo kwamadayi ku-substrate, kungcono ukomisa indwangu ngemva kokupakisha futhi ngaphambi kokuba idlulele enkambweni elandelayo.Izinto zokomisa ngokuvamile ukushisa kwe-infrared noma ngokusakazwa komoya oshisayo futhi kufanele zingathinteki ukuze kugwenywe ukumaka i-substrate nokungcoliswa kwezinto zokomisa.
Ngemuva kokumisa, udayi ufakwa kuphela ebusweni be-substrate;kufanele lingene ku-substrate ngesikhathi sesinyathelo sokulungisa futhi libe yingxenye ye-substrate ngokusabela kwamakhemikhali (odayi abasebenzayo), ukuhlanganisa (odayi be-vat nesibabule), ukusebenzisana kwe-ayoni (i-asidi nodayi abayisisekelo) noma isixazululo esiqinile (hlakaza odayi).Ukulungiswa kwenziwa ngaphansi kwezimo eziningana kuye ngokuthi udayi kanye ne-substrate ehilelekile.Ngokuvamile isitimu esigcwele ku-100°C sisetshenziselwa iningi lodayi.Odayi abahlakazayo bafakwa kuma-polyester substrates ngeNqubo ye-Thermasol lapho i-substrate ishiselwa khona ibe ngu-210°C isikhathi esingu-30-60 s ukuze odayi basakazeke engxenyeni engaphansi.Ngemva kokulungisa ama-substrates ngokuvamile ayawashwa ukuze kukhishwe udayi ongagxilile kanye nezinto ezisizayo.